Additive Manufacturing of Mechatronic Integrated Devices

This document was uploaded by one of our users. The uploader already confirmed that they had the permission to publish it. If you are author/publisher or own the copyright of this documents, please report to us by using this DMCA report form.

Simply click on the Download Book button.

Yes, Book downloads on Ebookily are 100% Free.

Sometimes the book is free on Amazon As well, so go ahead and hit "Search on Amazon"

In this dissertation a new process chain for the Additive Manufacturing of Mechatronic Integrated Devices (AMMID) is described, which provides a new way to manufacture 3-dimensional electronic devices based on the selective laser sintering (SLS) process using laser direct structuring (LDS) and metallization. The AMMID process chain meets the rising demand for highly functionalized parts, increasing individualization and shortening development cycles for electronic products.
The development for this process chain is based on an extensive literature review that indicates that an SLS-based process chain has great potential to produce 3-dimensional electronic devices with properties and with the future perspective of being suitable for an individualized mass production. The biggest, initial, technical hurdle is an unstable SLS process using a conventional LDS additive. The compound of SLS material and LDS additive was analyzed with DSC, which shows that the additive changes the melting behavior of the polymer by reducing the sintering window. A fine metal powder as an alternative additive affects the sintering window less and enables a stable process. To choose a suitable particle size and content for the metal powder an analytical material model is provided, that predicts the additive particle distribution within the material. This material model deepens the understanding of the activation mechanism during laser activation, provides hands-on information for powder preparation and it is applied for the design of the experiment for the development of the process chain with the new material.
Preliminary experiments are conducted along with the insights of the material model, which prove that redeposition is the main activation mechanism during laser activation with fine metal powders. Based on this, the process chain is developed, starting with a determination of a suitable additive content. A suitable material composition of a PA12 powder containing 2 wt.% of a copper powder with a mean particle diameter of 3.5 μm was identified. With regard to the laser activation, working laser parameters are developed (working parameter set feasible for all used post-process treatments: PRF = 1 kHz, dh = 25 μm, vs = 25 mm/s, tl = 20ns and P = 1.07 W). In this parameter development it is shown, that only closely located laser spots, enabling interaction of the laser pulses, are capable of activating the surface, while single laser pulses under applied conditions are not. By adding a post-process treatment as additional process step into the process chain, the quality of metallization and the size of design features could be improved. Chemical smoothing resulted in a complete reduction of unwanted metallization on non-activated surfaces. Conductor tracks with the minimal width of 300 μm could be realized. The process chain could be applied to demonstrator parts such as a drone housing and a PSU panel of an aircraft. Thus, this dissertation has raised the technology readiness level (TRL) from TRL2 to TRL6.
Finally, an economic consideration provides insights on the cost structure of parts produced with the AMMID process. A comparison of AMMID and injection molding shows economic viability for small lot sizes, 400 parts in case of the drone housing and 150 parts in case of the PSU panel. Finally, the analysis of the cost structure gives advice which future developments in the process chain have the greatest effect on costs and provides prioritization.

Author(s): Friedrich Wilhelm Proes
Series: Light Engineering für die Praxis
Publisher: Springer
Year: 2022

Language: English
Pages: 229
City: Cham

Abstract
Table of contents
List of figures
List of tables
List of acronyms
List of formula symbols
1 Introduction
1.1 Motivation and goal
1.2 History
1.3 Structure of this work
2 State of the art
2.1 Additive manufacturing technologies
2.2 Selective laser sintering
2.2.1 Data preparation
2.2.2 System components
2.2.3 Machine and powder preparation
2.2.4 Process
2.2.5 Post process
2.2.6 Part properties
2.2.7 Cost
2.3 3D Electronics
2.4 LDS process
2.4.1 Injection molding
2.4.2 Laser activation
2.4.3 Electroless plating with copper
2.4.4 Placement and interconnection
2.4.5 Market & Applications
2.4.6 ADDIMID
2.4.7 Cost
2.5 Additively manufactured electronics (AME)
2.5.1 SLS-based approaches for AME
2.5.2 Stereolithography (SLA)
2.5.3 Fused Filament Fabrication (FFF)
2.5.4 Inkjet
2.5.5 Dispensing
2.5.6 Aerosol-Jet printing
2.5.7 Plating
2.5.8 Miscellaneous
2.6 Knowledge gap
3 Preliminary considerations
3.1 Choice of the additive
3.2 Activation mechanism
3.3 Material model
3.3.1 Dependency of volume and weight content
3.3.2 Particle distribution
3.3.3 Deviation of a limiting copper concentration
3.3.4 Determination of a working copper concentration
3.3.5 Copper concentration at activation
3.4 Experimental proof of the activation mechanism
3.5 Surface roughness
4 Experimental development of the AMMID process
4.1 Experimental strategy
4.2 Description of Experiments
4.2.1 Determination of copper content
4.2.2 Activation mechanism for a single pulse
4.2.3 Activation by pulse interaction
4.2.4 Process window for laser activation parameters
4.2.5 Post-Process treatment
4.2.6 Design restrictions
4.2.7 Material properties
4.3 Materials, methods and systems
4.3.1 Materials
4.3.2 Methods
4.3.3 Systems
4.4 Experimental execution
4.4.1 Determination of copper content
4.4.2 Activation mechanism for a single pulse
4.4.3 Activation via pulse interaction
4.4.4 Process window for laser activation parameters
4.4.5 Post-Process treatment
4.4.6 Design restrictions
4.4.7 Material properties
4.5 Experimental results and discussion
4.5.1 Determination of copper content
4.5.2 Activation by a single pulse
4.5.3 Activation by pulse interaction
4.5.4 Process window for laser activation parameters
4.5.5 Post-Process treatment
4.5.6 Design restrictions
4.5.7 Material properties
5 Cross-sectional investigation
5.1 Alternative material
5.2 Transfer to alternative additive manufacturing technologies
5.3 Laser System
6 Application and economic viability of the AMMID process chain
6.1 Demonstrators
6.1.1 Drone
6.1.2 PSU Panel
6.2 Economics
6.2.1 Cost
6.2.2 Quality
6.2.3 Time
7 Summary
8 Outlook
References